Silicon monoxide vapor generated from Si/SiO 2 mixed‐powder compacts was used with NH 3 to synthesize silicon nitride in a tubular flow reactor operated at temperatures in the range of 1300°‐1400°C. The ammonolysis of SiO with excess NH 3 was very rapid, yielding three different types of silicon nitride at different longitudinal locations in the reactor: amorphous nanophase powder of an average size of about 20 nm, amorphous whiskers of a few micrometers in diameter, and α‐polycrystals. The amorphous products were heat‐treated for crystallization at temperatures between 1300° and 1560°C in a stream of dissociated NH 3 , N 2 , or N 2 /H 2 mixture gas. When dissociated NH 3 was used, nanophase powder was crystallized at 1300°C. The yield of nanophase silicon nitride from SiO varied from 13% to 43%, depending on operating conditions.