Answers are grounded in this paper and cite their sources.
In the presence of carbon or silicon carbide, silica can be reacted to form a vapor of silicon monoxide. The rates of these reactions were explored at 1300° to 1550°C. For mixtures of carbon and silica, evidence supported a two‐step reaction: silicon carbide formed prior to reaction between silicon carbide and silica.
No takes yet. Share an insight, caveat, or question.
Miller et al. (1979) studied this question.