This is the authors' abstract. We don't add key points for this paper.
Two methods were proposed and implemented for the fabrication of channel waveguides in an Er-doped Tellurite glass. In the first method, channel waveguides were fabricated by implanting 1.5 MeV and 3.5 MeV energy N+ ions through a special silicon mask to the glass sample at various fluences. Those waveguides implanted at a fluence of 1.0 × 1016 ions/cm2 operated up to 980 nm, and showed green upconversion of the Erbium ions. In the second method, channel waveguides were directly written in the Er3+: TeO2W2O3 glass using an 11 MeV C4+ ion microbeam with fluences in the range of 1 · 1014–5 · 1016 ions/cm2. The waveguides worked in single mode regime up to the 1540 nm telecom wavelength. Propagation losses were reduced from the 14 dB/cm of the as-irradiated waveguides by stepwise thermal annealing to 1.5 dB/cm at λ = 1400 nm.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Bányász et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: