Broad-line NMR measurements in the 160 to 350°K range have been carried out on poly(L-proline) Form I and Form II. Dynamic shear measurements, using a torsion pendulum, were made on poly(L-proline) Form II in the 130 to 250°K. region. Both Form I and Form II show decreases in the NMR line width in the 190 to 280°K. range, and Form II has a mechanical loss peak at 175°K (0.4 cps). The motion responsible for these processes is discussed.