The abrupt changes in the linear expansion and dilatometric measurements of poly‐(ethylene terephthalate) near 70°C indicate that the transition may be first order. DTA and DSC data show the normal heat capacity change at 70°C, while annealing for for 30 min. at 110°C induces further molecular order. Rapid quenching of PET after heating to 120°C yields an amorphous sample and measurement by depolarized light transmission as the sample is reheated shows rapid crystallization occurring near 80°C. With the occurrence of shrinkage near 68°C and apparent recrystallization at slow heating rates by depolarized light analyses, further support is added to the first‐order character of this phase transition. Isothermal annealing for short times at temperatures between 50°C and 80°C produces further increases in molecular order. Cyclic and linear PET oligomers do not contribute to the occurrence of the 70°C transition.
No takes yet. Share an insight, caveat, or question.
Gerald W. Miller (1975) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: