By thermal oxidation of 4H-SiC at 1150–1300 °C, the Z 1/2 and EH 6/7 concentrations can be reduced to below 1×10 11 cm -3 . By the oxidation, however, a high concentration of HK0 center ( E V + 0.78 eV) is generated. Additional annealing in Ar at 1550 °C results in elimination of the HK0 center. Thus, all the major deep levels can be eliminated by the two-step thermal treatment. Based on the depth profiles of deep levels, a model for the defect generation and elimination is proposed. The carrier lifetime in 4H-SiC epilayers has been improved from 0.64 (as-grown) to 4.52 µs by this method.