Answers are grounded in this paper and cite their sources.
The fabrication of multi-level SU-8 microstructures using multiple coating and exposure steps and a single developing step has been achieved for up to six layers of SU-8. Alternating layers of SU-8 2010 (thin) and SU-8 2100 (thick) photoresist films were spin coated, followed by soft-bake, ultraviolet (UV) exposure and post-exposure bake steps. The multiple SU-8 layers were simultaneously developed to create patterned microstructures with overall thicknesses of up to 500 µm and minimum lateral feature size of 10 µm. The use of a single developing step facilitated fabrication of complex multi-level SU-8 microstructures that might be difficult, or even impossible, to achieve by sequential processing of multiple SU-8 layers that are individually coated, baked, exposed and developed.
No takes yet. Share an insight, caveat, or question.
Mata et al. (2006) studied this question.