Seven prepolymers of phenol resin were decomposed into their monomers such as phenol, cresols, and p -isopropylphenol by reactions at 523−703 K under an Ar atmosphere in subcritical and supercritical water. The total yield of identified products depended on the kind of prepolymers, and the maximum yield reached 78% in the reaction at 703 K for 0.5 h. The decomposition reactions were accelerated by the addition of Na 2 CO 3, and the yields of identified monomers reached more than 90%. Two kinds of molding materials of phenol resin whose content of phenol resin was less than 50% were also decomposed mainly into phenol and cresols by the reaction in supercritical water.