SiC was synthesized via the gas‐phase reaction between SiO and CH 4 at 1500° and 1560°C in a tubular flow reactor. SiO vapor was generated from equimolar powder mixtures of Si and SiO 2 in the reactor while CH 4 was externally supplied. Products of different morphologies were collected at different longitudinal locations: whiskers, crystal aggregates, scale, and powder. The total yield of SiC, based on the amount of SiO generated, reached as high as 99%, of which 25–46% by mass was fine powder with sizes ranging from 60 to 300 nm.