Ti 3 SiC 2 joining has been successfully achieved by depositing a thin Cu or Zr layer on it and heat treating at low temperatures of 950° or 1100°C in an argon atmosphere, respectively, which are ∼500°C lower than the previous solid solution joining method. X‐ray diffraction and scanning electron microscope analyses reveal that a continuous Cu 3 Si or Zr‐silicide layer forms at the joint interface through the outward diffusion of Si atoms from the Ti 3 SiC 2 substrate into the deposited Cu or Zr layer. The strength of joints is evaluated by tensile bond‐strength test and 4‐point bending test methods. The Ti 3 SiC 2 /Cu/Ti 3 SiC 2 joints always fail from the substrate instead of from the bonding interface, while the Ti 3 SiC 2 /Zr/Ti 3 SiC 2 joints fail from the joint interface during tensile bond‐strength test. The 4‐point bending strength of Ti 3 SiC 2 /Cu/Ti 3 SiC 2 joints reaches a value of 238 MPa, which is 68% of the Ti 3 SiC 2 substrate. So joining using a Cu or Zr film as the interlayer followed by heat treating is a practical and efficient method for joining Ti 3 SiC 2 .
No takes yet. Share an insight, caveat, or question.
Li et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: