Answers are grounded in this paper and cite their sources.
We report on the preparation of amorphous (a-) insulators with the highest saturation induction ever achieved. Samples of a-(1 − x)BiFeO3−xABO3 (AB=PbZr, PbTi, BaTi) with x=0–0.6 were prepared by rf sputtering techniques. As-deposited films are x-ray amorphous and are paramagnetic. Films annealed in air at temperatures Ta=400–750 °C develop a magnetic moment. The room-temperature magnetization M increases with Ta and shows a maximum for a specific Ta value which is a function of the nature and amount of the nonmagnetic substitution. With further increase in Ta, the observed decrease in M is accompanied by the onset of crystallization in the films. The largest saturation induction, 4πMs = 3.8 kG, is observed for samples substituted with 0.5 PbZrO3. The Curie temperatures are in the range 380–440 °C and are well below the crystallization temperature.
No takes yet. Share an insight, caveat, or question.
Rao et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: