Answers are grounded in this paper and cite their sources.
In this study, blue-color emitting phosphors CaMgSi2O6:Eu2+ (CMS:Eu2+) were synthesized by the polymerizable complex method at 1000 °C in a reducing atmosphere. After the synthesis, the desired CMS crystals were obtained, but a small amount of impurity phases, such as Ca2MgSi2O7 and Ca3MgSi2O8, were contained. By adding lithium carbonate Li2CO3 as a flux to the polymerizable complex method and washing with 1 mol dm−3 HCl solution, the desired CMS:Eu2+ was obtained in a single phase. The maximum luminescence intensity was obtained at a flux concentration of 8 mol % for the composition CaMgSi2O6 when the amount of added flux was varied.
No takes yet. Share an insight, caveat, or question.
Taira et al. (2021) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: