Answers are grounded in this paper and cite their sources.
Electrical properties of a low-resistive and stable p-type ZnSe crystal grown by the temperature difference method under controlled vapor pressure are reported. The temperature dependence of Hall mobility, carrier (hole) concentration, and conductivity are measured by the van der Pauw method. Hole mobility appears to be about 200 cm2/V s at 100 K and about 50 cm2/V s at 300 K. The activation energy of a shallow acceptor impurity is also determined to be 70–85 meV.
No takes yet. Share an insight, caveat, or question.
Nishizawa et al. (1986) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: