Tellurium thin-film triodes were formed on quartz substrates which exhibited gain-bandwidth-products up to 170 MHz. Gain-bandwidth-products of 50 MHz and one-watt dissipation capabilities were exhibited by tellurium TFT's formed on sapphire substrates.