Fe14Nd2C (Φ) shows structural and intrinsic magnetic properties comparable to Fe14Nd2B. The phase Fe14Nd2C is found in long-time-annealed samples only (≳20 d at 850 °C) because of nucleation difficulties and slow growth kinetics. Compared to the Fe-Nd-B system the phase relations in the Fe-Nd-C system are unfavorable to produce sintered or even as-cast magnet materials, as manifested in the phase diagram presented. Fe14Nd2C is in equilibrium with either ferromagnetic and/or very corrosive phases, therefore the pure Fe-Nd-C material is useless. This situation can be changed by the addition of several elements to the Fe-Nd-C material: boron (even in small amounts of ≊0.05 mass %) accelerates the formation of Φ and reduces annealing times from weeks to hours; Cu added in the correct amount leads to new phase relations between Φ and NdxCuy intermetallic compounds. These intermetallics are nonmagnetic and low melting. Starting from as-cast material using the knowledge about the influences of substituants on phase relations and kinetics, a heat treatment can be chosen that leads directly to an isotropic, magnetically hard material with a rather small grain size (≲20 μm) and coercivities up to 1 T. The magnetization is comparable to isotropic Fe-Nd-B materials.
No takes yet. Share an insight, caveat, or question.
Grieb et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: