Answers are grounded in this paper and cite their sources.
Thin CoNiCr/Cr films (candidates for longitudinal recording media) were deposited on Corning 7059 glass substrate by RF diode sputtering. The CoNiCr layer thickness was fixed at 40 nm; the Cr layer thickness, d/sub Cr/, ranged between 60 and 400 nm. At d/sub Cr/=170 nm, when the substrate temperature before deposition, T/sub s/, was set below 100 degrees C, both the Cr underlayer and the CoNiCr layer were more or less randomly oriented. When specimens were deposited at T/sub s/>or=200 degrees C, the Cr layer was strongly [100] textured and the CoNiCr layer exhibited a strongly preferred texture. This CoNiCr texture is epitaxially favored by the Cr [100] texture. With increasing d/sub Cr/ the Cr [110] texture increased and the CoNiCr texture decreased. The grain size increased with T/sub s/ and d/sub Cr/. In-plane coercivity, H/sub c/, initially increased with T/sub s/ to peak at T/sub s/=200 degrees C. As T/sub s/ was increased further from 200 to 260 degrees C, H/sub c/ decreased. The squareness and saturation magnetization were not sensitive to T/sub s/.>
No takes yet. Share an insight, caveat, or question.
Duan et al. (1990) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: