Epitaxial Pb(ZrxTi1 - x)O3 films with 200 nm and 2 μm thickness were grown by metal organic chemical vapor deposition. Crystal symmetry changed from tetragonal to rhombohedral with increasing x value in Pb(ZrxTi1 - x)O3 [x = Zr/(Zr+Ti)] for both film thickness and a region for the co-existence of the mixture of tetragonal and rhombohedral exists around x = 0.5, becoming a little wider with increasing film thickness. Saturation and remanent polarizations (P sat and P r ) showed a minimum near x = 0.5 irrespective of the film thickness. The P r /P sat ratio also showed a minimum in case of 200 nm thick films, but such a minimum in P r /P sat was not observed in case of 2 μm thickness. Relative dielectric constant showed a maximum near x = 0.5 for both film thickness, but the effective longitudinal piezoelectric constant did not show any noticeable maximum near x = 0.5 irrespective of the film thickness, differently from the reported data for the sintered body.
No takes yet. Share an insight, caveat, or question.
Yokoyama et al. (2009) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: