Thin oxide films have been grown by anodization of GaAs in the negative glow region of a dc oxygen discharge. As-grown and annealed films grown on both p- and n-type bulk GaAs were characterized by conventional electrical measurements and by Auger analysis. The anodic oxide displayed ohmic characteristics up to fields of 0.5×106 V/cm with a resistivity of 1014 Ω cm in the as-grown condition and over 1015 Ω cm after anneal. Capacitance–voltage measurements indicated a fixed positive charge in the insulator of 1.5×1012 cm−2 for p-type substrates and 4.0×1011 cm−2 for n-type substrates. Majority carrier trapping near the oxide/GaAs interface was reduced by annealing and a corresponding reduction of As at the interface was observed. The distribution of fast interface states on p-type substrates had a broad minimum of 7–10×1011 cm−2 eV−1 near midgap while the distribution of fast interface states displayed a peak of over 1013 cm−2 eV−1 near midgap on n-type samples. No corresponding difference in the Auger composition profiles were observed between n- and p-type samples.
No takes yet. Share an insight, caveat, or question.
Chesler et al. (1978) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: