This is the authors' abstract. We don't add key points for this paper.
Persistent spectral hole burning was performed on the 7F0–5D1 transition of Sm2+ in thin films of SrFCl. Depending on the substrate and the growth conditions, a total hole depth between 47% and 70% was reached. The holes were Lorentzians of width 4(±0.3) cm−1. The time evolution of the hole depth was studied. It is described by two exponentials: a short time decay (t1=0.37 days) and a long time decay (t2=20.4 days) with a 20% infinite time limit. One- and two-photon burning mechanisms act.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Schnieper et al. (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: