Answers are grounded in this paper and cite their sources.
The 0–3 piezoelectric composites were prepared using a dielectric gel with 70 vol% of coprecipitated PbTiO 3 powders with sizes of 12 to 1100 nm. Composites were cured at 80°C for 10 h and poled with E = 0 to 100 kV /cm for 0 to 15 min at 85°C. X‐ray diffraction patterns taken on the surface of the composites before and after poling indicated that saturation poling was nearly achieved at 80 kV /cm. d̄ 33 was strongly dependent upon the particle size. Composites of fine PbTiO 3 powders, smaller than 200 nm, needed a much longer poling time to saturate than large particles probably because of the rotation of the single‐domain crystallites during poling.
No takes yet. Share an insight, caveat, or question.
Lee et al. (1989) studied this question.