This is the authors' abstract. We don't add key points for this paper.
The crystalline and electrical properties of W films are studied with regard to their relation to Ar sputtering pressure. An α‐W phase is formed at a pressure below 5 × 10 − 2 torr , and its density is 19.2 g/cm 3 , independent of the pressure. Above 5 × 10 − 2 torr , the β‐W phase and WO 3 are detected by x‐ray diffraction, and the oxygen and carbon are detected by SIMS. The RIE etching rate is found to be independent of the pressure for the α‐W phase. This rate increases with Ar pressure after β‐W phase formation, and the etching characteristic suffers from aging after deposition. Resistivity is found to be related to density rather than grain size. The W ‐ GaAs Schottky characteristics are somewhat influenced by the pressure. Degradation in carrier density, barrier height, and dark current caused by sputtering damage can be recovered by annealing.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Susa et al. (1985) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: