To realize high areal density, hard disk drives larger than 4 Tbit in−2, ultrafine FePt grains of less than 5 nm and grain density larger than 24 T in−2 are required. Although there have been many investigations to reduce the grain size of FePt, there are only a few reports on the control of grain density. To increase the grain density, we focused on three aspects of the surface morphology and grain density: nucleation sites on the substrate surface, surface free energy, and lattice mismatch. We achieved 14 T in−2 by maximizing the number of nucleation sites in the FePt-C granular film and found that the surface free energy and lattice mismatch are crucial parameters for controlling the grain density.