Answers are grounded in this paper and cite their sources.
We observed a majority-carrier trapping level at Ev+0.45 eV in boron-doped silicon with a wide range of resistivities after being quenched from 900 to 1200 °C. The carrier capture cross section was measured to be 4×10−18 cm2. The activation energy for migration and defect formation energy were found to be 0.76±0.05 and 2.8±04 eV, respectively, consistent with that of the interstitial iron in silicon. However, we found a marked boron dependence, indicating that the nature of the defect processes may be complex.
No takes yet. Share an insight, caveat, or question.
Gerson et al. (1977) studied this question.