This is the authors' abstract. We don't add key points for this paper.
Chemical bonding of H to displacement defects and internal surfaces in Si has been investigated by infrared-absorption and nuclear reaction analysis techniques. A He implantation/anneal sequence was used to produce faceted voids which are retained to at least 800 °C in a buried layer as revealed by transmission electron microscopy. Hydrogen was injected into void layers by three different methods: ion implantation, plasma exposure, and H2 gas exposure. Infrared absorption by Si-H stretch modes with frequencies characteristic of monohydrides on (100) and (111) surfaces are observed for all methods of H injection, consistent with bonding on faceted void surfaces. Thermal stability of Si-H is higher on void surfaces than on other trapping sites. Displacement defects produced by H-ion implantation trap H but release it upon annealing for retrapping on voids. The Si-H absorption bands with frequencies characteristic of monohydrides on (100) and (111) surfaces anneal in parallel between 600 and 800 °C and in coincidence with the loss of total H measured by nuclear reaction analysis. Moreover, densities comparable to the total H density are estimated for void surface states and for Si—H bonds on void surfaces. It is inferred from these results that bonding of H on the void surfaces is energetically favored over H2 formation in the voids, and it is concluded that the 2.5±0.2 eV determined in a separate study of H release from buried voids is the Si—H bond energy descriptive of both (111) and (100) surfaces.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Stein et al. (1993) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: