Answers are grounded in this paper and cite their sources.
A plasma immersion ion implantation (PIII) process has been developed for realizing shallow doping profiles of phosphorus and boron in silicon using an in-house built dual chamber cluster tool. High Si etch rates observed in a 5% PH3 in H2 plasma have been ascribed to high concentration of H(α) radicals. Therefore, subsequent work was carried out with 5% PH3 in He, leading to much smaller etch rates. By optical emission spectroscopy, the radical species H(α), PH*2, and PH* have been identified. The concentration of all three species increased with pressure. Also, ion concentrations increased with pressure as evidenced by Langmuir data, with a maximum occurring at 0.12 mbar. The duty cycle of pulsed DC bias has a significant bearing on both the implantation and the etching process as it controls the leakage of positive charge collected at the surface of the silicon wafer during pulse on-time generated primarily due to secondary electron emission. The P implant process was optimized for a duty cycle of 10% or less at a pressure of 0.12 mbar with implant times as low as 30 s. Secondary ion mass spectroscopy showed a P dopant depth of 145 nm after rapid thermal annealing (RTA) at 950 °C for 5 s, resulting in a sheet resistance of 77 Ω/◻. Si n+/p diodes fabricated with phosphorus implantation using optimized PIII and RTA conditions exhibit Jon/Joff > 106 with an ideality factor of nearly 1.2. Using similar conditions, shallow doping profiles of B in silicon have also been realized.
No takes yet. Share an insight, caveat, or question.
Ray et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: