CrN powder consisting of granular particles of ∼3 μm has been prepared by self‐propagating high‐temperature synthesis under a nitrogen pressure of 12 MPa using Cr metal. Dense pure CrN ceramics and CrN/ZrO 2 (2Y) composites in the CrN‐rich region have been fabricated by hot isostatic pressing for 2 h at 1300°C and 196 MPa. The former ceramics have a fracture toughness ( K IC ) of 3.3 MPa ·m 1/2 and a bending strength (σ b ) of 400 MPa. In the latter materials almost all of the ZrO 2 (2Y) grains (0.36–0.41 μm) are located in the grain boundaries of CrN (∼4.6 μm). The values of K IC (6.1 MPa · m 1/2 ) and σ b (1070 MPa) are obtained in the composites containing 50 vol% ZrO 2 (2Y).