Two-stage melting of the dilute gels of poly(γ-benzyl l -glutamate) in benzene has been studied by differential scanning calorimetry, wide-angle X-ray diffraction, and small-angle X-ray scattering using synchrotron radiation. Differential scanning calorimetry measurements show that the traces on heating exhibit two endothermic peaks at about 25 °C and at about 31 °C, thereby indicating the melting of two types of aggregates, while those on cooling exhibit no exotherm even at 0 °C, thereby indicating a large thermal hysteresis. Wide-angle X-ray diffraction measurements show that the profiles yield little of interest other than diffuse halos from the solvent except a diffuse small-angle scattering, thereby indicating that the aggregates do not contain a solid crystalline phase but a crystal−solvate phase. Small-angle X-ray scattering measurements show that the two-stage melting of the aggregates can be attributed to a melting first of the bundles of three rods and then of the bundles of two rods and that, above the two-stage melting temperature, the gels transform into the dilute and isotropic solutions, in which the poly(γ-benzyl l -glutamate) stiff chains are randomly dispersed and do not interact with each other. We suggest that the intermolecular interactions causing the bundles to aggregate are induced by the solvent.
No takes yet. Share an insight, caveat, or question.
Izumi et al. (1998) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: