This is the authors' abstract. We don't add key points for this paper.
The effects of B/P ratio on microstructure, crystallization behavior and soft magnetic characteristics of Fe 83.5 Si 3 B 10- x P 2+ x Cu 1.5 ( x = 0, 3, 6 & 8 at.%) amorphous alloys were studied. The results of Mössbauer spectra indicate that B/P ratio significantly impact the microstructure of amorphous alloy. A decrease in the B/P ratio facilitates the formation of an amorphous precursor containing more α-Fe-like structure and Cu(P)-clusters. As the B/P ratio reduces, the saturation magnetic induction ( B s ) and the coercivity ( H c ) of the as-quenched Fe 83.5 Si 3 B 10- x P 2+ x Cu 1.5 amorphous alloy decreases. After annealing with a low heating rate (1 °C/s), the Fe 83.5 Si 3 B 4 P 8 Cu 1.5 alloy shows a low H c (≤ 10 A/m) in a broad temperature range. With the decrease of the B/P ratio, the sensitivity of the soft magnetic properties of the nanocrystalline alloys to the annealing heating rate decreases.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Huang et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: