The technique for the study of the inhomogeneous magnetisation components of domain walls by Lorentz microscopy [15] is extended to cover structures which are not stray-field-free. Permitted forms for the distributions of the inhomogeneous components are derived and variants of the forms of vortex structures are considered. Results are presented of the application of the technique to 90° and 180° walls in (001) nickel platelets with thicknesses in the range 530 to 4230 Å. Below the critical thickness for stripe domain nucleation (≈︁2800 Å), 90° walls exhibit a pure Néel structure, as do 180° walls in thicknesses up to about 1000 Å. In the thickness range 1000 to 2800 Å 180° walls conform closely to the predicted vortex structure [11, 12]. These 180° walls are found to be subdivided through changes in the vortex corresponding to the predicted variants. Structures are proposed for the junctions in the subdivided walls, one of which may contain a Bloch point. At thicknesses greater than approximately 2800 Å, stripe domains are found to seriously modify the wall structures.
No takes yet. Share an insight, caveat, or question.
Harrison et al. (1973) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: