Cd-free fluorescent InP/ZnS quantum dots (QDs) have attracted attention for use as color converters of liquid crystal displays. To protect InP/ZnS QDs from oxygen, which degrades them by photo-oxidation during excitation, we fabricated a transparent monolithic silica composite containing the QDs using an aqueous solution of tetramethylammonium silicate (TMAS) as a silica source. The TMAS solution was basic and readily dispersed the negatively charged QDs obtained by ligand exchange of 1-dodecanethiol for 3-mercaptopropionic acid (MPA). A highly transparent monolithic TMAS-derived silica composite containing the MPA-modified QDs (InP/ZnS-MPA@TMAS) was obtained from the aqueous QD dispersion through a sol–gel process. The photoluminescence (PL) quantum yield of InP/ZnS-MPA@TMAS was 21.7%. Changes in PL intensity under continuous 400-nm excitation were measured to evaluate the photostability of the QDs in InP/ZnS-MPA@TMAS. The PL intensity of InP/ZnS-MPA@TMAS was over 90% of the initial value after 180 min, while that of a reference polymethylmethacrylate film containing hydrophobic QDs decreased to 69%. The higher photostability of InP/ZnS-MPA@TMAS than that of the reference film was explained by the TMAS-derived silica acting as a gas barrier to protect the embedded QDs from photo-oxidation by oxygen in air.
No takes yet. Share an insight, caveat, or question.
Watanabe et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: