We studied the melt composition to obtain pit-free, highly Bi-substituted (BiLu)3Fe5O12crystals by the LPE method. It was confirmed that adding B2O3to the melt increases the equilibrium segregation coefficient of Bi K0(Bi), and we found that a decrease in garnet composition ratio R4acts to increase the growth rate dependence of the normalized effective segregation coefficient of Bi Keff(Bi)/ K0(Bi). It was also found that crystals with mirror-smooth surfaces could be obtained by adding Gd2O3to the melt. Using a melt with Gd2O3/Lu2O3≥ 1, the pits which usually appear in LPE growth of (BiLu)3Fe5O12were eliminated, and pit-free, highly Bi-substituted (BiLuGd)3Fe5O12crystals were obtained. The optical properties of 250 μm thick (BiLuGd)3Fe5O12crystals were measured in order to evaluate their applicability to optical isolators for use at 1.3 μm. A sufficient Faraday rotation of θF= -1800 deg/cm and an extinction ratio of -40 dB were obtained.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Matsuda et al. (1987) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: