Answers are grounded in this paper and cite their sources.
Poly(3‐hydroxybutyrate‐co‐3‐hydroxyvalerate)(PHBV)/poly(3‐hydroxybutyrate‐co‐4‐hydroxybutyrate) (P3/4HB) blend films were prepared by solvent‐cast method. The nonisothermal crystallization results showed that PHBV and P3/4HB are miscible due to a single glass transition temperature (Tg), which is dependent on blend composition. The isothermal crystallization results demonstrate that the crystallization rate of PHBV becomes slower after adding amorphous P3/4HB with 19.2 mol% 4HB, which could be proved through depression of equilibrium melt point (Tₘᵒ ) from 183.7°C to 177.6°C. For pure PHBV and PHBV/P3/4HB (80/20) blend, the maximum crystallization rate appeared at 88°C and 84°C, respectively. FTIR analysis showed that PHBV/P3/4HB blend films would maintain the helical structure, similar to pure PHBV. Meanwhile, with increasing P3/4HB content, the inter‐ and intra‐interactions of PHBV and P3/4HB decrease gradually. Besides, a lower elastic modulus and a higher elongation at break were obtained, which show that the addition of P3/4HB would make the brittle PHBV to ductile materials.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: