We demonstrate the successful fabrication of an almost defect free Si(001) surface by refining the standard annealing and flashing surface preparation method. On any desired samples, we can routinely fabricate a surface with defect densities lower than 0.1%, significantly reducing the defect density compared to surfaces fabricated by standard methodology.
No takes yet. Share an insight, caveat, or question.
Hata et al. (2000) studied this question.