Answers are grounded in this paper and cite their sources.
Calcium lignosulfonate was incorporated into rubber compounds based on styrene-butadiene rubber (SBR) and acrylonitrile-butadiene rubber (NBR) in amounts ranging from 10 to 60 phr. A sulfur-based curing system and a peroxide curing system consisting of dicumyl peroxide in combination with methacrylic acid zinc salt were used for cross-linking of the compounds. The aim of the work was to investigate the influence of lignosulfonate and curing system composition of the cross-linking process, morphology, physical-mechanical and dynamic-mechanical characteristics of the composites. The achieved results showed that peroxide cured composites demonstrated higher cross-link density, which was found not to be influenced by the content of lignosulfonate. The cross-link density of sulfur-cured composites was lower and showed a decreasing tendency with increasing amounts of the biopolymer. A lower cross-linking degree was reflected in a higher elongation at break and higher increase in the elongation at break of the corresponding composites. On the other hand, peroxide-cured composites exhibited a higher modulus M100 and higher hardness. The microscopic analysis revealed that co-agent in peroxide vulcanization contributed to the improvement of adhesion between the biopolymer and the rubber resulting in higher tensile strength of the equivalent composites. The higher cross-link density of peroxide-cured composites caused higher restriction of the chain segments' mobility, due to which these composites exhibited a higher glass transition temperature.
No takes yet. Share an insight, caveat, or question.
Kruželák et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: