The dielectric constant εc of poled tetragonal BaTiO3, is measured in the frequency range 0.1 to 6 GHz. The dielectric behaviour is sensitive to sample preparation and to the poling procedure, which may be attributed to difficulties in getting samples really free from 90°-domains. This may explain the different values for εc found in literature. In - as believed − 90°-domain free BaTiO3, a small dielectric dispersion (Δε ≈ 3) is observed at several 108 Hz, which is attributed to a domain clamping effect of remaining 180°-domains. A comparison is made between the measured microwave dielectric constant and values of εc deduced from Raman measurements.