High-resolution x-ray scattering measurements on heavily doped Si:As (5×{}10²¹ As cm^-3) show lattice compression relative to pure silicon, Δaa=-0.0019±0.0003, although extended x-ray-absorption fine-structure measurements show that the As-Si bond length is 0.06±{}0.02 {} greater than the usual Si-Si bond length. The overall lattice compression is attributed to increased population of conduction-band states which reduces Si-Si bond lengths. These measurements provide the first direct measurement of the hydrostatic deformation potential for the conduction-band edge in silicon, +3.3±{}0.7 eV.