Answers are grounded in this paper and cite their sources.
Carrier concentrations in doped InN, In0.37Ga0.63N, and In0.75Al0.25N layers are reduced by both F+ ion implantation to produce resistive material for device isolation, and by exposure to a hydrogen plasma. In the former case, post-implant annealing at 450–500 °C produces sheet resistances ≳106 Ω/⧠ in initially n+ (7×1018–3×1019 cm−3) ternary layers and values of ∼5×103 Ω/⧠ in initially degenerately doped (4×1020 cm−3) InN. The evolution of sheet resistance with post-implant annealing temperature is consistent with the introduction of deep acceptor states by the ion bombardment, and the subsequent removal of these states at temperatures ≲500 °C where the initial carrier concentrations are restored. Hydrogenation of the nitrides at 200 °C reduces the n-type doping levels by 1–2 orders of magnitude and suggests that unintentional carrier passivation occurring during cool down after epitaxial growth may play a role in determining the apparent doping efficiency in these materials.
No takes yet. Share an insight, caveat, or question.
Pearton et al. (1993) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: