Phase‐pure powders of stoichiometric BiFeO 3 have been prepared by mechanosynthesis. Ceramics sintered by either conventional heating in air or spark plasma sintering ( SPS ) followed by oxidative anneal in air are highly insulating at room temperature with resistivity, extrapolated from the Arrhenius plots, of ~10 16 Ωcm and activation energy 1.15(2) eV, comparable with those of a good‐quality BiFeO 3 single crystal. By contrast, the as‐prepared SPS sample without the postsinter anneal shows lower resistivity, e.g., ~10 10 Ωcm at 25°C and activation energy 0.67(3) eV, indicating some reduction in the sample by the SPS process. The reason for the high conductivity reported for some ceramic samples in the literature remains unclear at present.