Answers are grounded in this paper and cite their sources.
Stoichiometric Pb(Mg 1/3 Nb 2/3 )O 3 perovskite ceramics produced by a reaction-sintering process are investigated. Without calcination, the mixture of PbO, Mg(NO 3 ) 2 and Nb 2 O 5 was pressed and sintered directly with and without a 950°C/2 h stage. Stoichiometric PMN ceramics of 100% perovskite phase are obtained after 1200–1270°C sintering with a 950°C/2 h stage. Without the 950°C/2 h stage, 100% perovskite phase PMN ceramics are also obtained after 1 h, 2 h and 4 h sintering at 1250°C and 1270°C. PMN ceramics with density 8.09 g/cm 3 and K max 19900 under 1 kHz are obtained by a reaction-sintering process.