Answers are grounded in this paper and cite their sources.
The influence of low temperature curing on the performance of concrete containing metakaolin (MK) is investigated. Portland cement was partially replaced with 0–30% MK. The water to binder ratio was maintained at 0.5 for all mixes. Concretes were subjected to water and air curing at 5°C. Compressive strength was conducted on water cured specimens whereas, ultrasonic pulse velocity and length change were conducted on water and air cured specimens. During the first day of hydration, the concrete strength is substantially reduced especially at high MK content. However, the incorporation of up to 20% MK causes an enhancement in concrete strength beyond 7days of curing. This increase could be up to 50% depending upon the age of curing and the MK content. After 28days of curing the relative strength continues to increase. This finding is compared with results obtained in a previous investigation for MK concrete cured at 20°C and analyzed using the maturity method. The incorporation of up to 15% MK causes an increase in linear shrinkage. Beyond 20% MK, the shrinkage is reduced.
No takes yet. Share an insight, caveat, or question.
Jamal Khatib (2009) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: