Answers are grounded in this paper and cite their sources.
Upon consecutive heat treatments at increasing temperatures, the microstructure of solution–sol–gel‐derived stannic oxide (SnO 2 ) xerogel evolves in three stages: (I) below 300°C, characterized by extensive dehydroxylation and gel shrinkage with little grain growth and surface loss; (II) between 300° and 500°C, by extensive crystallization, leading to dramatic surface loss (by 70%); and (III) above 500°C, by grain growth. Concurrently, the UV‐absorption edge shows red shifts during stages I and II and blue shifts during stage III, resulting in distinct color variations. The edge displacement bears a close correlation with a Raman “defect band” at ∼305–328 cm −1 .
No takes yet. Share an insight, caveat, or question.
Wu et al. (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: