Human bone mineral is different in composition from stoichiometric hydroxyapatite (Ca 10 (PO 4 ) 6 (OH) 2 ) in that it contains additional ions, of which CO 3 2- is the most abundant species. Two macroporous carbonate-substituted hydroxyapatite (CHA) scaffolds were prepared by treating a macroporous CaCO 3 column (porosity, 88%; pore and hole size, 160 and 71 μm), prepared in this study, hydrothermally at 120 °C in 1 M phosphate solutions of (NH 4 ) 2 HPO 4 and K 2 HPO 4 . Especially, it was found that the CaCO 3 was transformed into CHA after hydrothermal treatment (HT) for 24 h irrespective of the type of phosphate solution. Under HT for 24 h, the crystallite size and crystal shape of CHA prepared in K 2 HPO 4 solution (KCHA) and those of CHA prepared in (NH 4 ) 2 HPO 4 (NH 4 CHA) were quite different from each other. Moreover, NH 4 CHA contained 2.09 wt % A-type CO 3 2- out of 6.05 wt % CO 3 2-, but KCHA contained a small amount of A-type CO 3 2- (0.08 wt % out of 8.24 wt % CO 3 2- ). The chemical formulas were Ca 9.23 (NH 4 ) 0.12 (PO 4 ) 5.36 (CO 3 ) 0.64 (OH) 0.54 (CO 3 ) 0.34 for NH 4 CHA and Ca 8.18 K 0.5 (PO 4 ) 4.72 (CO 3 ) 1.28 (OH) 0.1 (CO 3 ) 0.02 for KCHA. Therefore, the properties, such as carbonate type and content, and crystal shape, of CHA are significantly affected by the type of phosphate solution.
No takes yet. Share an insight, caveat, or question.
Lee et al. (2008) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: