In this paper, we report the obtention of gadolinium oxide doped with europium (Gd2O3:Eu+3) by thermal decomposition of the Gd(OH)3:Eu3+ precursor prepared by the microwave assisted hydrothermal method. These systems were analyzed by thermalgravimetric analyses (TGA/DTA), X-ray diffraction (XRD), structural Rietveld refinement method, fourrier transmission infrared absorbance spectroscopy (FT-IR), field emission scanning electron microscopy (FE-SEM) and photoluminescence (PL) measurement. XRD patterns, Rietveld refinement analysis and FT-IR confirmed that the Gd(OH)3:Eu3+ precursor crystallize in a hexagonal structure and space group P6/m, while the Gd2O3:Eu3+ powders annealed in range of 500°C and 700°C crystallized in a cubic structure with space group Ia-3. FE-SEM images showed that Gd(OH)3:Eu3+ precursor and Gd2O3:Eu3+ are composed by aggregated and polydispersed particles structured as nanorods-like morphology. The excitation spectra consisted of an intense broad band with a maximum at 263 nm and the Eu3+ ions can be excitated via matrix. The emission spectra presented the characteristics transitions of the Eu3+ ion, whose main emission, , is observed at 612 nm. The photophysical properties indicated that the microwave sintering treatment favored the Eu3+ ions connected to the O-Gd linkages in the Gd2O3 matrix. Also, the emission in the Gd2O3:Eu3+ comes from the energy transfered from the Gd-O linkages to the clusters in the crystalline structure.
No takes yet. Share an insight, caveat, or question.
Moura et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: