Georgia kaolinite dehydroxylated at 950°C for 24 h, then leached with KOH at 90°C for 1 h, shows a well‐resolved 29 Si MAS NMR resonance at −77.5 ppm, within 2 ppm of the calculated position for Si incorporated in γ‐alumina spinel. From a knowledge of the total SiO 2 in the leached sample and its partitioning between the spinel and residual grain boundary phases, a maximum of 3.9 wt% is estimated to be present in the spinel.