Answers are grounded in this paper and cite their sources.
This research work presents the synthesis of ZnAl 2 O 4, samarium doped ZnAl 2 O 4 : x%Sm 3+ ( x = 1–11mol%) and co-doped ZnAl 2 O 4 : x%Sm 3+ , A n+ ( x = 5mol%, A n+ = Na + , Mg 2+ , Bi 3+ ) nano phosphors. All prepared samples are calcinated at an optimized temperature of 900 ⁰ C. Powder XRD studies reveal that all synthesized samples are crystallized in cubic phase, with Fd-3 m space group, matches with JCPDS # 05–0669. The ZnAl 2 O 4 : Sm 3+ exhibits major excitation peaks at 274, 306, 346, 377, 404, 418, 442 and 466 nm. Inquiringly, we perform photoluminescence studies under the excitation of 274 nm and 404 nm. With 404 nm excitation, the emission peak intensity of ZnAl 2 O 4 : x% Sm 3+ ( x = 1–11 mol%) achieves its maximum when the doping concentration is 5 mol%. Charge compensators effect of different valance cation co-dopants (A n+ = Na + , Mg 2+ , Bi 3+ ) on the PL emission intensity is further optimized at the concentration of 2 mol% for 274 nm excitation. CIE1931 color coordinates for ZnAl 2 O 4 :5mol% Sm 3+ :2mol%Mg 2+ phosphor, (0.656, 0.343), closely approximate those of an ideal orange-red light emitting phosphor (0.670, 0.333). Measurements reveal that the average decay time for ZnAl 2 O 4 :5mol% Sm 3+ and ZnAl 2 O 4 :5mol% Sm 3+ : Mg 2+ 2mol% is 0.98 ms and 0.057 ms, respectively. This paper also summarizes the typical behavior of ZnAl 2 O 4 and its Cr 3+ association when excited by 404 nm light, for researchers interested in zinc aluminates.
No takes yet. Share an insight, caveat, or question.
Kempaiah et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: