Answers are grounded in this paper and cite their sources.
Borosilicate glass powder with simulated high‐level radioactive waste (HLW) was solidified by a hydrothermal hotpressing method. A leach test of the solid bodies was performed. Twenty‐one elements composing the simulated HLW in the leachant were analyzed quantitatively by neutron activation analysis. The addition of Al(OH) 3 , up to 7.5% of the starting powder, reduced the leachability. The first densification of the starting powder during hydrothermal hot‐pressing takes place by the rearrangement of particles, followed by solution‐precipitation. The densification fits two types of rate equations. Activation energies obtained from two rate equations agree and are smaller than those of the glass without simulated HLW. The results indicate that simulated HLW in the starting powder acts to reduce the activation energy for densification during hydrothermal hot‐pressing.
No takes yet. Share an insight, caveat, or question.
NISHIOKA et al. (1990) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: