Interconnected porous Pb (Zr0.53 Ti0.47)O3 ceramics, with controlled porosity up to 0.73, were prepared. The piezoelectric coefficient, 933, measured using a resonant method and a Berlincourt d33 meter increased as the porosity increased. The d33 and 933 of the porous PZT ceramic/ silicone rubber composite were almost the same as that of porous PZT.