Answers are grounded in this paper and cite their sources.
The mechanism of pyrolysis of silicon carbide fibre (Nicalon) has been investigated at temperatures from 1673 to 1973 K under an argon atomsphere. The rate of pyrolysis was measured by means of thermogravimetry, and the formation of the pyrolysis product was examined by chemical analysis and TEM observation.The rate of pyrolysis depends on temperature. The mass loss measured was attributable to both SiO and CO gas evolved by the pyrolysis. During pyrolysis, the three-dimensional growth of the cristallite of SiC was observed in the fibre. As a result, the amorphous fibre was crystallized in β-SiC.The rate of pyrolysis was described by the Avrami-Erofeev equation. The order of this equation was m=1.3. The Arrhenius plots of the rate constants gave the apparent activation energy of 484 kJ/mol. These results showed that the rate was controlled by the crystal growth of SiC involving the diffusion of carbon in the fibre.
No takes yet. Share an insight, caveat, or question.
Shimoo et al. (1990) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: