Answers are grounded in this paper and cite their sources.
Novel polyenamines with inherent viscosities in the 0.2–1.1 range were synthesized by the vinylogous, nucleophilic substitution polymerization of 1,6‐diethoxy‐1,5‐hexadiene‐3,4‐dione with aromatic and aliphatic diamines in polar aprotic solvents at room temperature. The most effective polymerization medium was hexamethylphosphoramide for preparing high‐molecular‐weight polymers from aromatic diamines. The dilute solutions showed a marked decrease in viscosity with time. The aromatic polyenamines began to lose weight around 200°C under thermogravimetric analysis in air and nitrogen.
No takes yet. Share an insight, caveat, or question.
Ueda et al. (1978) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: