Answers are grounded in this paper and cite their sources.
The effect of Fe and B 4 C on the sintering behavior and mechanical properties of TiB 2 ceramics have been studied. Sintering was performed in an Ar atmosphere at 2000° using attrition‐milled TiB 2 powder (mean particle size = 0.8 μm). When a small amount of Fe (0.5 wt%) was added, abnormal grain growth occurred and the sintered density was low. In the case of B 4 C added along with 0.5 wt% Fe, however, abnormal grain growth was remarkably suppressed, and the sintered density was increased up to 95% of theoretical. But with excess Fe addition (5 wt%), B 4 C grains did not act as a grain growth inhibitor, and B 4 C grains were frequently trapped in large TiB 2 grains. The best mechanical properties were obtained for the TiB 2 –10 wt% B 4 C–0.5 wt% Fe ceramics, which exhibited a three‐point bending strength of 400 MPa and a fracture toughness of 5.5 MPa · m 1/2 .
No takes yet. Share an insight, caveat, or question.
Kang et al. (1989) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: